Print Back
AMS-5510, ASTM-A-240

Physical Properties
  • Minimum Tensile Strength (0.002 to 0.003" Thick) - 70 to 110 ksi
  • Minimum Tensile Strength (0.003 to 0.004" Thick) - 70 to 105 ksi
  • Minimum Tensile Strength (Over 0.004" Thick) - 70 to 100 ksi
  • Minimum Yield Strength (0.2% Offset) - 25.0 ksi
  • Elongation in 2 Inches (0.002 to 0.003" Thick) - 20%
  • Elongation in 2 Inches (0.003 to 0.004" Thick) - 30%
  • Elongation in 2 Inches (Over 0.004" Thick) - 40%
  • Minimum Hardness - No Req.
Unit of Measure

Specifications

Width

N/A 24 in

Length

N/A 36 in

Alloy

N/A T321 Stainless Steel Alloy

Thickness

N/A 0.0060 in

Thickness Tolerance

N/A 5 %

American Society for Testing and Materials (ASTM) Steel Standard

N/A ASTM-A-240

Aerospace Material Specification (AMS)

N/A AMS-5510

Alloy Steel Type

N/A Stainless Steel

Material Form

N/A Sheet

Temper

N/A Annealed Temper

Chemical Composition

Maximum Carbon Composition

N/A 0.08 %

Maximum Manganese Composition

N/A 2.00 %

Maximum Silicon Composition

N/A 1.00 %

Maximum Phosphorus Composition

N/A 0.04 %

Maximum Sulfur Composition

N/A 0.03 %

Maximum Chromium Composition

N/A 19.00 %

Maximum Nickel Composition

N/A 12.00 %

Maximum Titanium Composition

N/A 0.70 %

Maximum Molybdenum Composition

N/A 0.75 %

Maximum Copper Composition

N/A 0.75 %

Maximum Nitrogen Composition

N/A 0.10 %

Chemical Composition Table

N/A

Physical Properties

Minimum Tensile Strength (0.002 to 0.003 Inch (in) Thick)

N/A 70 to 110 ksi

Minimum Tensile Strength (0.003 to 0.004 Inch (in) Thick)

N/A 70 to 105 ksi

Minimum Tensile Strength (Over 0.004 Inch (in) Thick)

N/A 70 to 100 ksi

Minimum Yield Strength (0.2 Percent (%) Offset)

N/A 25.0 ksi

Minimum Elongation in 2 Inch (in) (0.002 to 0.003 Inch (in) Thick)

N/A 20 %

Minimum Elongation in 2 Inch (in) (0.003 to 0.004 Inch (in) Thick)

N/A 30 %

Minimum Elongation in 2 Inch (in) (Over 0.004 Inch (in) Thick)

N/A 40 %