Print Back
AMS-5519, ASTM-A-666

Physical Properties
  • Minimum Tensile Strength - 185 ksi
  • Minimum Yield Strength (0.2% Offset) - 140 ksi
  • Elongation in 2 Inches (Up to 0.0150" Thick) - 8%
  • Elongation in 2 Inches (Over 0.0150" Thick) - 9%
  • Minimum Hardness - 41 HRC (Product shall not be rejected on the basis of hardness if tensile properties … are acceptable)
Unit of Measure

Specifications

Width

N/A 24 in

Length

N/A 36 in

Alloy

N/A T301 Stainless Steel Alloy

Thickness

N/A 0.0151 in

Thickness Tolerance

N/A 0.001 in

American Society for Testing and Materials (ASTM) Steel Standard

N/A ASTM-A-666

Aerospace Material Specification (AMS)

N/A AMS-5519

Alloy Steel Type

N/A Stainless Steel

Material Form

N/A Sheet

Temper

N/A Full Hard Temper

Chemical Composition

Maximum Carbon Composition

N/A 0.15 %

Maximum Manganese Composition

N/A 2.00 %

Maximum Silicon Composition

N/A 1.00 %

Maximum Phosphorus Composition

N/A 0.04 %

Maximum Sulfur Composition

N/A 0.03 %

Maximum Chromium Composition

N/A 18.00 %

Maximum Nickel Composition

N/A 8.00 %

Maximum Molybdenum Composition

N/A 0.75 %

Maximum Copper Composition

N/A 0.75 %

Chemical Composition Table

N/A

Physical Properties

Minimum Tensile Strength

N/A 185 ksi

Minimum Yield Strength (0.2 Percent (%) Offset)

N/A 140 ksi

Minimum Elongation in 2 Inch (in) (Up to 0.0150 Inch (in) Thick)

N/A 8 %

Minimum Elongation in 2 Inch (in) (Over 0.0150 Inch (in) Thick)

N/A 9 %
Minimum Hardness1 N/A 41 Rockwell C
  • 1 Product shall not be rejected on the basis of hardness if tensile properties are acceptable